How To Choose A Carbon Raiser
Poor-quality recarburizers can cause significant losses to enterprises, including slower absorption, lower absorption rates, increased costs, unnecessary waste, and the presence of harmful elements that affect product quality, leading to further losses.

High-temperature fully graphitized low-sulfur recarburizer has low sulfur and nitrogen content, effectively preventing nitrogen porosity defects. It performs well for high-end castings that require strict control of sulfur and nitrogen indicators, offering high absorption rates, low impurities, and stable composition. With proper use, the absorption rate can reach approximately 95%.
Medium-temperature graphitized recarburizer offers relatively high cost-effectiveness and can be used in the melting process of ordinary nodular cast iron and gray cast iron. With proper use, the absorption rate can reach ≥90%.

Semi-graphitized recarburizer is mainly used for gray cast iron castings. It can also be used for ordinary nodular cast iron products that require a small amount of recarburizer in the melting charge. During the melting process, it should be added before two-thirds of the molten iron is melted. With proper use, the absorption rate can reach ≥90%.
High-sulfur recarburizer is a non-graphitized type that is not subjected to high-temperature treatment during production. It has relatively higher sulfur and nitrogen content compared to graphitized recarburizers and is suitable for gray cast iron products, as it can reduce the amount of sulfur iron added. The absorption rate of this recarburizer ranges from 85% to 90%, and its melting absorption speed is relatively slow, making it unsuitable for addition in the later stages of molten iron melting.