The Influence of Carbon, Sulfur, and Nitrogen Content on Recarburizers and Castings
When using a recarburizer as a conditioning material, the carbon, sulfur, and nitrogen elements it contains can significantly impact the final casting.

Carbon is a fundamental element in cast iron and exists primarily in two forms: free carbon (graphite) and combined carbon (cementite). Carbon is a strong graphitizing element. Increasing the carbon content increases the quantity of graphite, but it can also coarsen the graphite flakes. Conversely, reducing the carbon content results in finer graphite particles. The higher the fixed carbon content of the recarburizer, the higher the carburizing efficiency, the faster the dissolution rate in the molten iron, and the higher the absorption rate. However, if the initial carbon content of the molten iron is too high, the absorption rate of the recarburizer slows down, the amount absorbed decreases, oxidation loss increases, and the overall recovery rate decreases. The carbon content directly affects the microstructure and mechanical properties of the casting.

Sulfur stabilizes cementite and hinders graphitization in castings. A small amount of sulfur dissolves in ferrite and cementite as elemental sulfur, reducing the solubility of carbon in liquid cast iron. Most sulfur exists in the form of iron sulfide (FeS) and other sulfide inclusions. Iron sulfide has a low melting point and is soft and brittle, which reduces the strength of cast iron and causes hot shortness (a tendency to form hot cracks).
An appropriate amount of nitrogen (approximately 60–120 ppm, or expressed as mL/100g) can shorten graphite length, increase its curvature, blunt its ends, reduce its aspect ratio, promote a pearlitic matrix, and improve the tensile strength and hardness of the casting. However, if the nitrogen content is too high, it can easily lead to fissure porosity (nitrogen gas hole defects) in the casting.